Step 2: Crack Repair

Before applying an Ultra Surface Polymer Concrete texture coat or 1/4" Stamping application, all structural moving cracks should be repaired with the Ultra Surface Crack Repair System as shown below.

(Note: For the 1/4" Stamping System only, the expansion joints will also need to be repaired with this crack repair system, and then cut back open the day after stamping.)

Fig. 1
Clean cracks during surface preparation.

Fig. 2
Clean cracks during surface preparation.

Fig. 3
Scrape excess Epoxy off the surface.

Fig. 4
Apply Elastomeric Basecoat over crack repairs.

Fig. 5
Immediately apply 4" Crack Repair Fabric over the Elastomeric Basecoat while still wet.

Fig. 6
Immediately apply another coat of Elastomeric Basecoat over the 4" Crack Repair Fabric.

Fig. 7
Apply a patch coat of Ultra Surface Polymer Concrete over the crack repairs. This step is not necessary when doing 1/4" Stamping.

Go To Step 1 2 3 4 5
Intro Procedure Products Stamps Colors Photos



© 2004-2008 Concrete Solutions Inc., 3904 Riley St. San Diego CA, 92110


Built/Hosted by ESP Design Studio Inc
For a quick view of our systems go to concrete resurfacing
Visit our new Concrete Countertop web site concrete countertop